Stockpile of type C materials on areas Kutai Barat estimated about 6,01 million tons, with total area of the region 31.628,70 km2, implementation of this research is to determine the properties of the utilization crushed stone Sendawar on Asphalt Treated Base mixture. Sand Tenggarong which is located in river Mahakam is estimated has stockpile of material 156 million m3, with total area of the region 27.263,10 km2 . Implementation of this research to determine the properties of the utilization the sand of Tenggarong on Asphalt Treated Base mixture. This research is performed by using volumetric and Marshall characteristics which consist of density, Voids in the Mineral Aggregate (VMA), Voids In The Mix (VITM), Voids Filled With Asphalt (VFWA), stability, flow, and Marshall Quotient as parameters. With the index value of immersion or residual strength.Physical data which can be used experiments is 24,22 % for viscosity of asphalt aggregate, 2,618 % for specific gravity bulk coarse aggregate, 1,561 % for absorption, 2,635 % for specific gravity bulk medium aggregate, 1,851 % for absorption, 2,569 % for specific gravity bulk fine aggregate, and 0,616 % for absorption. Mean while data the sand aggregate’s experiments is 2,569 % for specific gravity bulk and 0,916 % for absorption. Based on Marshall Test, the optimum content asphalt are is 6,500 %. The index value of immersion is 96,941 %.
Keyword: Split Melak, Sand Tenggarong, Asphalt Treated Base (ATB), Marshall Quotient